Brief Description: 5-min epoxy hardpoints into landing gear bulkheads
The foam was trimmed with a utility knife to accommodate the hardpoint shapes. The shop, foam, and hardpoints were vacuumed to clean up the fiberglass dust. The temperature in the shop was 88 deg F and the humidity was reduced to 44% using a dehumidifier. 5-minute epoxy was used to fix all 4 hardpoints into the foam shapes for the landing gear bulkheads.