Date:  7-2-2013
Number of Hours:  1.25
Manual Reference:  ch 25
Brief Description:  sanding the skim coat

I followed Cory Bird's advise and wet sanded with a long sanding block and 150 gritl and I'm happy with the results. Exactly what I was looking for today was low spots and boy are there a lot. The good news is that I'm almost certain that High Build Primer will get everything evened out. I'm now researching High Build Primers as I'm torn between rolling or spraying. More later....