Wet sanded MLG doors, baggage door and other small pieces.
Attempted to prime upper cowling. On first pass of paint gun got the same blistering as before. Stopped after one small pass.
Primed both ailerons, MLG doors, NLG doors, oil door, oil drain door and several other small pieces. The priming came out perfectly so I continued on with color after a one hour flash time.
All pieces came out in acceptable condition...maybe even good condition. Now, if I could just figure out the problem with the cowling...