The first round of micro was sanded down and another layer added. 160 g resin was made into dry micro paste. In preparation for the next layer, I realized that the epoxy chart that I was using for the West 105 resin/206 hardner was incorrect. It was calculating a 6:1 ration. The resin is supposed to be a 5:1.