Spent some time in front of the telly ironing my remaining roll of peel ply. The cardboard tube at the core has collapsed, and everytime it is handled it creases up a bit more. Re-rolled it onto some 50mm PVC pipe, as the tube was toast.
Trial fitted LWA4/6 & W18 with standoffs, and all seems do-able.
After a break floxed (plans says micro) in LWA4 & W18, micro'd in LWA6. Bit more ding recovery and hardshelling with excess resin. I put a dam of plasticene under LWA4 to contain the flox. Apologies for working in my undies, but it was hot, and I had been drinking...
Captain underpaints inspecting installation over a lovely shiraz